Gravimetric Corrosion Tests and Surface Analysis of SUS 310S in Model Seawater
Md. Saiful Islam, Most. Sabina Yasmin, Masatoshi Sakairi
Journal of Materials Science Research and Reviews · pp. 22–30 · Published 14 Jan 2022
Abstract
The corrosion behaviors of SUS 310S in model seawater with different metal cations have been investigated by gravimetric tests and surface analysis. Different corrosion rates were observed in different solutions by the kinds of metal cations, and Zn2+ containing solution showed the lowest corrosion rate among used solutions. SEM observations showed the pits on the surface that were different from each other. White pits were observed on the specimen immersed in the Zn2+ containing solution. X-ray photoelectron spectroscopic results showed the presence of Zn2+ and Al3+ on the specimen immersed in the corresponding solution. Metal cations that have large X showed the tendency to form a fence layer on the specimen surface. Metal dissolution as well as chloride ions attacks were inhibited by the layer of metal cations with large X.
Cited by 0
No indexed citations yet.
Related research
- Morphological and Anti-microbial Study of Whey Protein Concentrate Prepared by Dehydrating Milk Serum — shares topic coverage
- Organoleptic and Morphological Analysis of Citrus Peel Powder — shares topic coverage
- Spore Morphology of 34 Species of Monilophyta from Northern Parts of Iran — shares topic coverage
- Synthesis and Characterization of Epichlorohydrin- Crosslinked Lumbang (Aleurites moluccana)-Derived Activated Carbon Chitosan Composite as Cr(VI) Bioadsorbent — shares topic coverage
- Mycotoxin and Fungal Contamination of Fresh and Dried Tomato — shares topic coverage
Article metrics
Real usage data collected on this platform.
17
Page views
0
PDF downloads
27
Outbound clicks
0
Citations
Views over time
Views by country
Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".
Traffic sources
Referring site, by host.
Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.