Characterization of Chitosan-Based Edible Films for Food Packaging Applications
Asif Ali T S, Sweety, Venkatesh M, Aarathy Bose, Aiswarya Velekat Santhosh
Journal of Advances in Biology & Biotechnology · pp. 166–175 · Published 10 Jan 2025
10.9734/jabb/2025/v28i11871Abstract
Aims: To study the optimization and characterization of chitosan-based edible films for food packaging applications Study Design: This study was experimental and conducted in a lab. Place and Duration of Study: The study was conducted at the Department of Dairy Technology, Dairy Science College, Hebbal, Bengaluru, Karnataka, India, between October 2022 and July 2023. Methodology: The edible film was developed with 9 different combinations by 3 concentrations of chitosan 1.50, 2.0 and 2.5% along with 3 concentrations of glycerol 0.5, 0.75 and 1%. Various characteristics like moisture content, water solubility, thickness, density, GSM, colour, transmittance, water vapor transmission rate (WVTR), tensile strength, elongation are assessed. The film was optimised on the basis of water vapor transmission rate, tensile strength and elongation. ANOVA was the method used for statistical analysis, and the significance between the control and sample was assessed using a critical difference (CD) at a 5% significance level. Results: Increase in chitosan concentration the film thickness, GSM, solubility and density increases whereas moisture content decreases. Increase in glycerol concentration the film thickness, GSM, moisture, solubility increases but there was decrease in film density. The film colour parameters lightness L*, redness a* and yellowness b* increase as chitosan content increases, whereas transmittance decreases. Increased glycerol content increased the film's colour parameters redness a* and transmittance, but had no influence on the film's yellowness whereas as the lightness value decreases. The film made with 2.5% chitosan and 0.5% glycerol has the lowest water vapour transmission rate, 10.70 g/m2h. The tensile strength of film made with 2.5% chitosan and 0.5% glycerol has the highest value of 18.56 MPa. Film produced using 1.5% chitosan and 1% glycerol has the highest value of 51.73% elongation. Conclusion: Increasing the concentration of chitosan improves tensile strength but reduces elongation. On the other hand, adding more glycerol lowers tensile strength but increases elongation. A film containing 2% chitosan and 0.75% glycerol is considered the best choice, offering a balanced water vapor transfer rate, tensile strength, and elongation.
Cited by 1
1 citation reported by external sources — individual citing-article records aren't available to list yet.
Related research
- Susceptibility of Some Clinically Resistant Bacterial Isolates to Thyme Essential Oil, Chitosan and Lactobacillus reuteri — shares topic coverage
- Effects of Addition of TiO2 Edible Coatings and Storage Periods on the Chicken Eggs Quality — shares topic coverage
- Gelatin, Chitosan, and Beeswax Based Edible Packaging for Food Product: A Review — shares topic coverage
- Functional Edible Coating from Banana Peel Starch (Musa sapientum L.) and Vannamei Shrimp Shell Chitosan for Quality Maintenance of Tomato — shares topic coverage
- Effect of the Different Surface Coatings and Packaging Materials for Shelf Life and Quality of Guava (Psidium guajava L.) CV. Allahabad Safeda — shares topic coverage
Article metrics
Real usage data collected on this platform.
0
Page views
0
PDF downloads
0
Outbound clicks
1
Citations
Views by country
Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".
No views recorded yet.
Traffic sources
Referring site, by host.
No traffic recorded yet.
Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.