The Influence of Multiple Welding Repairs of Pipelines in Residual Stress Assessment Related to Stress Corrosion Cracking
A. Contreras, S. L. Hernández, R. Galvan, O. Vega
Current Journal of Applied Science and Technology · pp. 621–634 · Published 9 Jan 2015
10.9734/BJAST/2015/14931Abstract
The effect of residual stress of multiple welding repairs in seamless API 5L X52 on the stress corrosion cracking (SCC) susceptibility was evaluated. Four repairs of the girth weld were evaluated through X-ray diffraction (XRD) on the internal face of the pipe to measure residual stresses in longitudinal and circumferential direction. Residual stresses in the circumferential and longitudinal direction reach values of about 77% and 58% of the UTS (460 MPa) respectively, approaching to the YS of the steel (360 MPa). It was observed that its magnitude increases as move away from weld center line. SCC susceptibility of X52 steel welded joints with the residual stresses generated was evaluated through slow strain rate tests (SSRT) in a soil solution at low and high pH. Relation between mechanical properties and residual stresses on the SCC susceptibility was analyzed. SCC index obtained from the mechanical properties of SSRT indicate good SCC resistance of X52 steel exposed to soil solution at low and high pH. From these results, it is suggested that the region with high residual stresses before to generate cracks in the steel surface due to the combination of soil solution and the strain applied, should favor pitting formation and not cracking. Initiation of micro-cracks from these pits will depend on the geometrical form of the pit and the stresses state can be established at given pitting. It is suggested that initiation of micro-cracks from these pits may depend on the dissolution rate and morphology of the pitting and stresses on the bottom of the pitting. This favorable condition could appear increasing the soil exposition time of the steel and reducing the strain rate applied on the SSRT.
Cited by 17
Mohammad Shojaati, Seyed Farshid Kashani Bozorg, Masoud Vatanara · International Journal of Pressure Vessels and Piping · 2020
Shidong Wang, Lyndon Lamborn, Karina Chevil · Corrosion Science · 2020
Shidong Wang, Hamed Shirazi, Hanan Farhat · Corrosion Science · 2024
Shidong Wang, Lyndon Lamborn, Karina Chevil · Corrosion · 2021
Shidong Wang, Lyndon Lamborn, Weixing Chen · Corrosion Science · 2022
Shidong Wang, Weixing Chen · Corrosion · 2022
Wenqian Zhang, Kewei Fang, Yujin Hu · Corrosion Science · 2016
Sampath S.S., Nethri Rammohan, Reema Shetty · World Journal of Engineering · 2016
Showing 8 of 17 known citations — external sources report more than can currently be individually listed.
Related research
- Statistical Evaluation of the Effect of Process Parameters on the Depth of Penetration of Tungsten Inert Gas Arc Cladding Weld in Mild Steel — shares topic coverage
- Analysis of Corrosion Behaviour of Welded Austenitic Stainless Steel Immersed in Aqueous Alkaline Medium — shares topic coverage
- Evaluation of Occupational Lead Exposure in Informal Work Environment in Kenya — shares topic coverage
- Bibliometric Analysis of Publications on “Hazards and Health Effects Associated with Welding” From 2010 – 2023 — shares topic coverage
- Optimization of Mild Steel Welding Process Parameters Using Multivariate Linear Regression — shares topic coverage
Article metrics
Real usage data collected on this platform.
59
Page views
0
PDF downloads
7
Outbound clicks
17
Citations
Views over time
Views by country
Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".
Traffic sources
Referring site, by host.
Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.