Skip to content
Research Article Open access CC BY 4.0

Development of a Set-up for Creep Test of Biological/Viscoelastic Materials Subjected to Uniaxial Compressive Loading

Aaradhana Patel, Mohan Singh, Avinash Kumar

Current Journal of Applied Science and Technology · pp. 1–9 · Published 15 Jun 2018

10.9734/CJAST/2018/42055

Abstract

A set-up was developed for testing of creep test of viscoelastic materials like vegetables, fruits etc. creep test was provided under in uniaxial compressive loading.  If a constant load is applied to biological materials and if stresses are relatively large, the material will continue to deform with time, this slow deformation with time is known as creep.  Green pea kernels were taken in the set-up for testing of creep. Set-up is consisted of a PVC cylinder, two SS plates, a rectangular wooden box, A stand is provided to facilitate mounting of scale for measurement of downward movement of cover plate inside the cylinder. seven different compressive stresses 88.55, 177.11, 265.66, 354.22, 442.77, 531.33 and 708.44 N/m2 were used and deformation was observed at different time intervals 0, 0+,5, 10, 15, 20, 45, 60, 90, 120 and 150 minutes. Creep curves were plotted to show the variation in volumetric strain for different time intervals. The volumetric strain with respect to variation of loading is maximum in case of maximum stress that was 708.44 N/m2.

Creep test viscoelastic materials compressive stresses volumetric strain creep curves

Cited by 0

No indexed citations yet.

Article metrics

Real usage data collected on this platform.

38

Page views

0

PDF downloads

7

Outbound clicks

0

Citations

Views over time

Views by country

Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".

Traffic sources

Referring site, by host.

Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.