The Influence on Synthetising Mg-Al Hydrotalcite by Using Different Mg and Al Sources as the Precursors
Miao Niu, Mande Qiu, Qingjiao Han, Yidan Wang
Chemical Science International Journal · pp. 1–7 · Published 20 Jul 2016
10.9734/ACSJ/2016/27767Abstract
In this paper, Mg-Al hydrotalcite crystals were synthesized using the different Mg sources and Al sources as the precursor via hydrothermal method. The effects of different Mg and Al sources on the microstructure and the growth of LDHs were investigated by the X-ray diffraction (XRD), scanning election microscopy (SEM) and energy dispersive spectrometer (EDS), simultaneity. Besides, according to the ligand theory, its growth mechanism was discussed. The research indicated that the better LDHs crystal could been prepared under the condition of pH=12, hydrothermal temperature of 120°C and time of 12 h. The different Mg and Al sources combination had certain influence on the phase, dispersion, regularity, ratio of thickness, purity, size and microstructure of LDHs products. When the Mg sources was fixed for MgCl2, choosing Al2O3, Al(NO3)3 and AlCl3 as Al sources respectively, the obtained LDHs with poor purity, regularity dispersion and crystallinity were synthesized when Al2O3 was used as Al sources; but the LDHs had better regularity, dispersion, crystalline and purity when Al(NO3)3 and AlCl3 were chosed as Al sources. The reason could be that the different solubility and polarity of anion caused the slight variation of products microstructure. Compared to MgCl2 with high dissolvability, when the Mg sources was fixed for Mg(NO3)2, choosing Al(NO3)3 and AlCl3 as Al sources respectively, it is more advantageous to getting LDHs with better crystalline, regularity, and smaller in size. When both Mg sources and Al sources had higher solubility, the synthesized LDHs were with higher crystalline and regularity. The EDS analysis results showed that the purity of LDHs synthesized with Al2O3 had poor solubility. In addition, LDHs prepared by Mg sources and Al sources with higher solubility do not contain any other anionic impurities, and the average ratio of Mg/Al is about 3, which is very close to the theoretical value.
Cited by 2
Graciele Vieira Barbosa, Maria Aparecida Zaghete, Rafael Aparecido Ciola Amoresi · Materials Sciences and Applications · 2017
Tian Huiyuan, Cui Jiehu, Cui Baoyu · Journal of Water Process Engineering · 2024
Related research
- Adamantane-Functionalized Phthalimide Scaffold: Pathways to Supramolecular Interactions and Drug Discovery — shares topic coverage
- Synthesis and Structure of 6-Acetyl-2-Arylhydrazone Derivatives of Thiazolo[3,2-a]Pyrimidine — shares topic coverage
- Luminescence of the Conjugate Bases of [2-(2-Hydroxyphenyl)phenyl]phosphinic Acid and Single-Crystal X-Ray Structure Determination of Sodium [2-(2-Hydroxyphenyl)phenyl]phosphinate — shares topic coverage
- Synthesis of Bipyridine Ether-Type Bifunctional Precursors — shares topic coverage
- Remarkable Influence of Structures around Rhenium (V) Centers Constructed in Polyoxotungstates for Methanol Dehydrogenation under Visible Light Irradiation — shares topic coverage
Article metrics
Real usage data collected on this platform.
0
Page views
0
PDF downloads
0
Outbound clicks
2
Citations
Views by country
Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".
No views recorded yet.
Traffic sources
Referring site, by host.
No traffic recorded yet.
Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.