Examining the Application of Coating Methodologies and Surface Analysis Post- machining Low Carbon Steel
Osei Asibey, Baidoo Phillip, Richard K. Fiator, Frederick Adu Wireko, Alexander Yaw Osei
Journal of Engineering Research and Reports · pp. 123–135 · Published 2 Apr 2025
10.9734/jerr/2025/v27i41461Abstract
This study explored the corrosion behaviour of low carbon steel under various coating methods and engineered machining techniques. The study successfully created coatings with strong adhesion and minimal porosity using electroplating, painting, and blackening methods. To evaluate the corrosion resistance of these coatings, the research conducted tests using hydrochloric acid (HCL), sodium chloride solution (NaCl) and freshwater (H2O), as well as mechanical scratch tests to assess the coatings' interaction with the steel substrate. The experiment used low carbon steel specimens and analyzed their corrosion behaviour over a five-week period. The results showed that the all coatings exhibited superior corrosion resistance in freshwater (H2O), while blackening and electroplating performed better in hydrochloric acid (HCL) and sodium chloride solution (NaCl). Notably, paint coatings showed significant surface removal, while electroplating and blackening coatings displayed strong bonding and no visible removal. The study concluded that electroplating and blackening are more suitable for low carbon steel applications requiring mechanical strength due to their ability to withstand scratches without compromising surface integrity. The findings highlight the varying effectiveness of different coating methods in protecting low carbon steel from corrosion in different environments.
Cited by 0
No indexed citations yet.
Related research
- High Hardness Nickel - Carbon Nanotubes Composite Electroplating — shares topic coverage
- Electronic Behaviour of Schottky Diodes Fabricated from Electroplated CdSe Semiconductors — shares topic coverage
- Investigating Wear Behaviour of Multiple Layer Copper Coating on 3D-Printed Biodegradable PLA Composite — shares topic coverage
- Design and Development of a Modernized Cassava Grating Machine — shares topic coverage
- Comparative Optimisation of the Cutting Parameters for Surface Quality and Energy Efficiency during the Machining Manufacturing of Teak, Saligna and Pine Wood Materials — shares topic coverage
Article metrics
Real usage data collected on this platform.
56
Page views
0
PDF downloads
19
Outbound clicks
0
Citations
Views over time
Views by country
Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".
Traffic sources
Referring site, by host.
Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.