10.9734/ajocs/2020/v8i419056Abstract
Polycrystalline alloys based on cobalt and elaborated by classical foundry are known since the middle of the last century. They are currently still used, notably for geometrically complex components working at high temperature. Beyond the oldest ones reinforced by chromium carbides, new principles of carbides–strengthened cobalt–based alloys have recently appeared. MC–type refractory mono–carbides allow maintaining the melting start temperature at a high level when they are present as single carbide phase. Their high temperature stabilities and script–like morphologies also favor high mechanical properties at elevated temperatures. Optimized MC–carbides fractions can be obtained with carbon contents, close to 0.4 wt.%C, for achieving significant strengthening without threat for the low and high temperature toughness. Controlling the carbon content is thus of prior importance. Unfortunately the most common metallographic apparatus used for measuring the chemical composition of alloys – the Energy Dispersion Spectrometers (EDS) attached to Scanning Electrons Microscopes (SEM) – are not able to analyze, with sufficient accuracy, carbon with so low contents. A simple indirect method using both EDS and SEM is proposed here to get some information about the carbon content in several MC–reinforced Co–based superalloys.
References (3)
- 1 Superalloys: a technical guide
- 2 As-Cast Microstructures and Hardness of Chromium-Rich Cobalt-Based Alloys Reinforced by Titanium Carbides
- 3 Microstructure and hardness of several chromium-containing Co-based alloys reinforced by MC (TaC, NbC or HfC) carbides in as-cast or heat-treated conditions
Cited by 8
Shuo Chen, He Jiang, Fa Wang · JOM · 2026
L. Fenocchio, A. Saviot, S. Gambaro · Journal of Materials Research and Technology · 2025
He Jiang, Fa Wang, Jia-Ji Dong · Social Science Research Network · 2023
P. Berthod, Assane Kane, L. Aranda · Canadian metallurgical quarterly · 2021
He Jiang, Fa Wang, Jianxin Dong · Journal of Materials Research and Technology · 2023
Showing 5 of 8 known citations — external sources report more than can currently be individually listed.
Related research
- Morphological and Anti-microbial Study of Whey Protein Concentrate Prepared by Dehydrating Milk Serum — shares topic coverage
- Organoleptic and Morphological Analysis of Citrus Peel Powder — shares topic coverage
- Spore Morphology of 34 Species of Monilophyta from Northern Parts of Iran — shares topic coverage
- Synthesis and Characterization of Epichlorohydrin- Crosslinked Lumbang (Aleurites moluccana)-Derived Activated Carbon Chitosan Composite as Cr(VI) Bioadsorbent — shares topic coverage
- Mycotoxin and Fungal Contamination of Fresh and Dried Tomato — shares topic coverage
Article metrics
Real usage data collected on this platform.
70
Page views
0
PDF downloads
30
Outbound clicks
8
Citations
Views over time
Views by country
Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".
Traffic sources
Referring site, by host.
Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.