Applications of Titanium Alloys, Ni-Based Superalloys, and Aluminum Alloys in Powder Bed Fusion Additive Manufacturing: Process–Microstructure–Property Relationships, Defect Engineering, and Emerging Frontiers
Journal of Materials Science Research and Reviews · pp. 932–953 · Published 24 Sep 2026
10.9734/jmsrr/2026/v9i4521Abstract
Powder bed fusion (PBF) additive manufacturing has emerged as a transformative near-net-shape fabrication technology for advanced metallic components across aerospace, biomedical, energy, and automotive sectors. This review establishes a processing-defect-microstructure-performance tetrahedron framework to systematically evaluate how laser powder bed fusion (LPBF) and electron beam powder bed fusion (EB-PBF) parameters govern the structural integrity and functional properties of six alloy families, with primary emphasis on titanium alloys, nickel-based superalloys, and aluminium alloys, while retaining ferrous alloys, copper alloys, and refractory metals as concise comparative cases. The thermal processing history is examined as the primary control dimension that deterministically shapes defect formation, microstructural evolution, and mechanical performance. Defect mechanisms spanning lack-of-fusion porosity, keyhole porosity, and cracking are analysed through a progressive hierarchy from energy-driven universal phenomena to material-specific manifestations. Microstructural control strategies, including solidification morphology engineering, phase transformation pathway manipulation, and grain boundary design, are synthesised across alloy systems. The mechanical performance hierarchy reveals that Ti-6Al-4V and nickel superalloys deliver the highest specific strength and creep resistance but exhibit greater sensitivity to defect-induced fatigue scatter, while 316L stainless steel and AlSi10Mg offer superior process robustness at moderate strength levels. Advanced characterisation techniques, in-situ monitoring capabilities, and multiscale simulation frameworks are surveyed as essential enablers for process qualification. Emerging frontiers in multi-material architectures, alloy design exploiting non-equilibrium solidification, and industrial scalability are critically assessed, identifying key knowledge gaps and future research directions toward qualification-ready PBF manufacturing.
Cited by 0
No indexed citations yet.
Related research
- Co-authorship Networks in Additive Manufacturing Studies Based on Social Network Analysis — shares topic coverage
- Biomedical Implant Materials in Transition: Recent Developments, Clinical Applications and Future Perspectives — shares topic coverage
- Design and Analysis of the Impact of Ultraviolet Aging on the Mechanical Properties and Durability of PLA Lattice Structures — shares topic coverage
- Microleakage Evaluation of Two Different Fabricated Composite Inlays: An in vitro Study — shares topic coverage
- Additive Manufacturing in Food Systems: A Comprehensive Review of 3D-printed Meat Technology — shares topic coverage
Article metrics
Real usage data collected on this platform.
38
Page views
0
PDF downloads
4
Outbound clicks
0
Citations
Views over time
Views by country
Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".
Traffic sources
Referring site, by host.
Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.